Place of Origin: | China |
---|---|
Brand Name: | BODA |
Certification: | ISO9001:2015,ISO14001 |
Model Number: | BD-10502 |
Minimum Order Quantity: | 50kg |
Price: | US$51.80/kg-$53.50/kg EX-WORK |
Packaging Details: | 10kg per bottle or 50kg per drum |
Delivery Time: | 5-8 working days |
Payment Terms: | T/T |
Supply Ability: | 10-15 tons per month |
Color: | Dark Gray | Shape: | Spherical |
---|---|---|---|
Chemistry: | WC 12Ni | Service Temperature: | 500 ℃ Max |
Appliciation: | Ball Valves In Oxidizing Environments Gate Valves Oil Field Equipment Parts Used In Submerged Seawater Conditions | Size: | -53+20um -45+15um -45+11um -38+10um -30+10um -45+20um -45+5um -30+5um |
Highlight: | WC-12Ni HVAF Powders,Wear Resistant HVAF Powders,WC-12Ni Hardfacing powder |
Grade | Ct% | Ni% | Fe% | O% |
BD-10502 | 5.2-5.6 | 11.5-13.5 | <0.2 | <0.5 |
Specification & Physical Properties :
Spec. | Type | Size um | Equal to Woka | Apparent density g/cm3 |
Flow Rate s/50g |
Application |
BD-10502-1 |
WC-Ni 88/12 Agglomerated and Sintered |
53-20um | Woka 3401 | >4 | <18 | HVOF JP5000 JP8000/DJ2600 DJ2700/Jet Kote/Woka Jet/K2 |
BD-10502-2 |
WC-Ni 88/12 Agglomerated and Sintered |
45-20um | Woka 3406 | >4 | <18 | HVAF |
BD-10502-3 |
WC-Ni 88/12 Agglomerated and Sintered |
45-15um | Woka 3402 | >4 | <18 | APS |
BD-10502-4 |
WC-Ni 88/12 Agglomerated and Sintered |
45-11um | Woka 3403 | >4 | <18 | |
BD-10502-5 |
WC-Ni 88/12 Agglomerated and Sintered |
38-10um | >4 | <18 | ||
BD-10502-6 |
WC-Ni 88/12 Agglomerated and Sintered |
30-10um | Woka 3404 | >4 | <18 |
Introduction :
BODA WC-12Ni products are spheroidal, agglomerated and sintered powders for thermal spray containing a uniform distribution of 88 % tungsten carbide with medium sized carbide grains as a hard phase and 12 % nickel as a binder metal.
The finer powder particle size distributions produce very tough and dense coatings that can often be used in the “as-
sprayed” condition without post-coat finishing.Coatings made from tungsten carbide materials resist fret-
ting, abrasion, hammer and sliding wear. BODA WC-12Ni series products are most often used for abrasion-resistant coatings in dry environments. Their use at atmospheric temperatures
above 500 °C (930 °F) is not recommended to prevent oxidation of the tungsten carbide. The corrosion resistance of WC-Ni is generally better than that of WC-Co coatings in similar environments, but not as good as coatings of WC-Co-Cr. BODA WC-12Ni coatings exhibit higher hard-ness compared to coatings of WC-17Ni, but have lower toughness. They have lower hard-
ness but better toughness than coatings from WC-10Ni. The absence of cobalt allows
BODA WC-12Ni coatings to be used in radioactive environments.
HVOF coatings of these materials are dense, show good
bond strength and are more homogeneous than coatings
applied using atmospheric plasma spray or combustion
powder Thermospray ™ coatings.